Leyla,
Thanks for the tip!.  I will try this out next week.  Is this that you =
suggested an alternative to the Acetone stripping process?  And it is =
the AZ300 Stripper you are using?
=20
Jeffrey

________________________________

From: mems-talk-bounces@memsnet.org on behalf of Leyla Soleymani
Sent: Fri 3/23/2007 10:28 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Patterning Gold heaters on glass



Hi,

I do not do the lift off process, but for genereal resist removal. I =
heat up
the AZ stripper to about 80 degrees and leave my samples in it for 20
minutes. That removes all the resist. I hope this is helpful for your
process.

Regards,
Leyla