Hi, I am using PMMA A2 or PMMA A3 for ebeam lithography. In order to get a better BOE etch mask, I would liket to have a thick PMMA layer. Can I spin the PMMA multiple times? If so does anyone know if I should softbake and respin or spin multiple times before softbake? I would really appreciate your help. Regards, Leyla Soleymani University of Toronto