Hi all, in order to handle very thin silicon wafers (50um or less), i'm
looking for thermal release tape. Until now i've found only "REVALPHA",
www.nitto.com/product/datasheet/e_parts/010/index.html
any other suggestion about thermal release tape or any other solution to
handle very thin silicon wafers ?

Best regards,
Andrea