Thank you to everyone who replied to my previous e-mail! I will be ordering an UV filter this week and will try the same processes I did before with a filter and see if I will get any good results. Those 10 um holes I'm making are suppose to go all the way through 10 um thick layer of SU-8 2010 and stop on the SU-8 layer 2100 (100 um thick). Since I have already exposed the bottom layer it would be no problem to make these holes open through 10 um deep. The only problem I have is make these holes nicely open! The final three layer SU-8 structure will be a mold for PDMS and it is important to have 10um holes open. Speaking of using hot plates - I tried that, too, but didn't use slow ramping up or down during the bakes. I may have to try that. Thank you again to everyone and if you will have more advice for me I would greatly appreciate it. Anna