Hi Jeff, Yes, you can get >110 deg on PMMA using vapor deposited MVD coatings. In-situ deposited adhesion layers will help to attach hydrophobic silanes to PMMA material. Boris Kobrin, Ph.D. Director of Technology Applied Microstructures, Inc. 1020 Rincon Circle, San Jose, CA 95131 (408) 907-2885 x2805 boris_kobrin@appliedmst.com Message: 3 Date: Tue, 24 Apr 2007 15:04:53 -0400 From: "Jeff chen"Subject: [mems-talk] how to make the PMMA surface more hydrophobic? To: mems-talk@memsnet.org Message-ID: Content-Type: text/plain; charset=ISO-8859-1; format=flowed Hi, All, I am working to make the PMMA surface more hydrophobic, like the contact angle >90. Anyone has such experience?