durusmail: mems-talk: Re: Using carbon fibers
Re: Using carbon fibers
1998-06-29
Re: Using carbon fibers
Stefan Fiedler
1998-06-29
On Jun 23, 14:54, Tom Prigg wrote:
> Subject: Using carbon fibers
> I am interested in attaching some carbon fibers to a rat's whiskers
while
> moving across a texture of many fine contact circuts.  I am having
trouble with using different types of glue and was looking for
> some other alternatives.  Are there any suggestions?
>
> Thank you for any suggestions.
>
>
>-- End of excerpt from Tom Prigg

3M has a quickly curing adhesive ( 400 nm), used for dental construction
work: Multipurpose adhesive 7543, 3M Dental Products, St. Paul
should work

Good luck
S. Fiedler
********************************************************************
 Fraunhofer-Institut fuer               Dr. Stefan Fiedler
 Zuverlaessigkeit u. Mikrointegration   Telefon +49 (0) 30/46403-276
 Gustav-Meyer-Allee 25                  Telefax +49 (0) 30/46403-271
 13355 Berlin                           e-mail  fiedler@izm.fhg.de
 Germany
********************************************************************


reply