If the bond is good - no problem. If it's going to fall apart - the bond is bad. -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of kris Sent: Wednesday, May 09, 2007 5:32 PM To: mems-talk@memsnet.org Subject: [mems-talk] bonded wafers dice Hello, I was wondering if we can dice a Au-Au thermocompression bonded wafer pair using the diamond saw. I need individual dies from the wafer pair to go for the etch trails. Your suggestions are highly appreciated.