 David,
Is the film low stress? Can you share data regarding this?
Thanks

Shay

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of David Nemeth
Sent: Wednesday, May 09, 2007 6:09 PM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] Au electroplating

For thickness less than about 0.25 microns, you can use electroless gold:
http://www.transene.com/au.html  (For example)