It depends on the design, but with many acclerometers, a voltage change like that can result in a change in output of the device. We (Silicon Designs, Inc. www.silicondesigns.com) use this effect to simulate vibration and even high acceleration in our devices. If you have unknown fluctuations, then you are just adding to the noise of the device. --Jason Tauscher -----Original Message----- From: Xu Jun [mailto:engp7703@leonis.nus.edu.sg] Sent: Friday, June 26, 1998 9:13 PM To: MEMS@ISI.EDU Subject: microaccelerometer hello! i want to know the consequence if the voltage on electrode-plates (fingers) of a microaccelerometer is unstable (for example, changes between -5% and +5%)? best regards ***--------------------------------------*** Mr. Xu Jun Dept of MPE The National University of Singapore 10 Kent Ridge Crescent, Singapore 119260 E-mail:engp7703@leonis.nus.edu.sg ***--------------------------------------***