> I want to know how to make etchants of Nichrome which can be used with resist Transene makes (or made) a nichrome etchant which is likely patternable with photoresist. ****************************************** Kirt R. Williams, Ph.D. Research Staff Scientist Lucas NovaSensor 1055 Mission Ct., Fremont, CA 94539-8203 Kirt_Williams@compuserve.com (510) 661-6147 FAX (510) 770-0645 ******************************************