Hello Peter, We are using Karl Suss bonde 6BE for the Au Au thermocompression bonding. The bonding temperature is 400C for 1hr and 7500mbar of pressure is applied on the wafers. Good surface (O2 plasma cleaned), 2000A of Sio2 or TiW should act as a good diffusion barrier between the silicon and Au. Thanks, Kris