Hi All, I am looking for a process by which i can have around 50nm thick gold film on uncrosslinked SU-8. The process should be such that it does not croslinkes the SU-8 present. The substrate on which i am coating SU-8 is glass. Any suggestion to this would be highly appreciated. Thanks Nidhi Maheshwari PhD Student School of Biosciences and Bioengineering IIT Bombay India