Hi Shay, I am using straight developer. Lithography is done with a chrome mask. Herman. ________________________________ Van: mems-talk-bounces@memsnet.org namens Dave Verzonden: zo 10-6-2007 17:17 Aan: mems-talk@memsnet.org Onderwerp: [mems-talk] RE: 2.5 um microchannels in SU-8 (shay kaplan) Are you using straight developer from the bottle or a dilution? 2.5 microns is pretty damn small for near UV, i bet that the lithography process is your problem. Are you direct writing or are you using a photomask?