Dear MEMS community

I need to bond two pieces of silicon substrate together. They both have
electroplated gold of 17.6um. I wonder what would be a good way to bond them
together.

I've heard of thermal-compression bonding. Could someone recommend  some
good references to this method? Thanks

btw. my samples are small. they are about 6mm x 6mm

Best Regards

Leo