Hi; Maybe you have done wrong anything in your recipe. After your sample was spined, did you wait 3- 4 minutes to remove N2 in inside the resist. Tolga YELBOGA Project Engineer Nanotechnology Researh Center Bilkent University Bilkent, Ankara 06800 TURKEY Voice: 90-312-290-1020 www.nanotr.bilkent.edu.tr -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Rama Kotha Sent: Wednesday, June 20, 2007 12:25 AM To: mems-talk@memsnet.org Subject: [mems-talk] Smooth Side Wall Profile usin AZ-5209 *Smooth side wall profile Using AZ 5209* Hi, I am trying to develop a smooth side-wall profile (of step height ~ 2um) using AZ 5209 E positive resist. I have tried for different exposure and development times, and have obtained bumps along the sidewall. Could anyone suggest me, how to obtain a smooth side wall profile without curved edges.