Dymax has a uv adhesive that dissolves in water for temporary use. Use a
drop in three corners, align and once in place uv expose.

Shay

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of Kirt Williams
Sent: Thursday, July 12, 2007 8:50 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Mounting shadow masks

I have used cyanoacrylate (super glue) to hold on shadow masks.
Apply a fraction of a drop with a toothpick so you don't get too much.

To remove, heat above about 300 C and it decomposes, leaving a dust. Just
wipe it off.
Acetone or MEK at room temperature might also work for removal.

    --