durusmail: mems-talk: Ag deposition on Si
Ag deposition on Si
2007-08-21
2007-08-27
Ag deposition on Si
Kirt Williams
2007-08-27
See http://microlab.berkeley.edu/labmanual/chap1/JMEMSEtchRates2(2003).pdf .
Ag was evaporated onto Si at 0.5 nm/s. A 10-nm Cr adhesion layer was used.
    --Kirt Williams

----- Original Message -----
From: "Vikrant A. Chaudhari :)" 
To: 
Sent: Monday, August 20, 2007 9:33 AM
Subject: [mems-talk] Ag deposition on Si

> hello friends,
>
> has any one tried Ag deposition on Si
>
> vikrant
reply