Nb can be etched with SF6 plasma. For wet etch HF can be used. Roger Shile -----Original Message----- Hi all, Looking for some help on the kind of wet etchants available for etching Nb. I have vaguely heard about HF(1):HNO3(1). Does anybody have an idea of what is the etch rate of this chemical for Nb? Are there any other etchants available for Nb? And does it etch other metals like Au, Fe, CuMn, Ni? Thanks, ES...