Hi, I recommend to use an adhesion layer for Au, such as Cr or Ti. You can use the same with SU-8, but you do not need to. Regards, Silvan Yue Mun Pun, Jeffrey schrieb: > Hi, > Can anyone tell me how I can ensure SU-8 and gold conductors adhere well to glass wafer?