We believe we have observed a strong correlation of <100>:<1111> selectivity to loading. When we etch one wafer we get about ½ the selectivity as we do when we etch 25 or more. Is this a known phenom? Should we expect the selectivity to be effected this dramatically? We are talking about selectivities of >65:1 vs ~30:1. Steve