Hello, Plasma needs to be grounded properly otherwise, the flickering occurs. Now in case of sputtering of polymers, deposition of teflon etc etc causes the deposition of insulators on the walls and electrodes of the plasma source. This is one of the main reasons why the plasma flickers. You may run argon plasma for 1-2 hours to sputter clean all the surface. Nabhiraj Variable Energy Cyclotron Centre Dept Of Atomic Energy 1/AF, Salt Lake, Kolkata On Nov 13, 2007 5:08 AM, PRAMOD GUPTAwrote: > Hi > > Does any one know what could be the reasons for Plasma Flickering in Oxford Plasmalab 80 Plus RIE system?. I am trying to etch polymers with SF6/O2/CHF3 gas chemistry at 30mTorr, 200W. The recipe was working perfect earlier. Pure O2 plasma, even at 30mTorr, does not flicker at all. It starts flickering when you mix O2 with SF6 and/or CHF3. What could be the reasons?