Hello all,

What is correct protocol for cleaning a gold melt (for ebeam) when not in use?

Some of the suggestions that I have heard are:
(a) Immerse the melt in IPA when not in use
(b) No need to immerse it, but clean it using a fabwipe & IPA before use
(c) Hands off the melt. No need to clean it.


All comments & suggestions are welcome.

Thanks,
Shivalik