Hi Dave, a possible way of doing that is repeating plasma oxidation cycle followed by an wet etching with a dilueted HCl solution. Therefore you are etching layer of about 0.5 nm per cycle, it is a bit fastidious but the uniformity is great and the RMS identical to the initial one. Cheers, Abdou.