You can buy wafer dicing saw blades and put them onto milling machines. Its not elegant but it does work. Regards, Steven J. Adamson President IMAPS Market Manager, Asymtek -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of R.Loiacono@surrey.ac.uk Sent: Wednesday, February 06, 2008 8:50 AM To: Haixin.Zhu@asu.edu; mems-talk@memsnet.org Subject: RE: [mems-talk] Dicing saw Following this post, I have the same problem. I have been looking on the internet for a long time, but basically dicing saws (for silicon, in my case) are really bulky, big and expensive. It would be nice to have a dicing saw that can just be put on a table for cutting wafers or dicing smaller samples. Any suggestions?