durusmail: mems-talk: Wafer silicon smoothing surface
Wafer silicon smoothing surface
2008-02-07
2008-02-10
2008-02-12
Wafer silicon smoothing surface
Andrea Mazzolari
2008-02-10
Try to look at "Improved anisotropic deep etching in KOH-solutions to
fabricate higly specular surfaces", Microelectronic Engineering 57–58
(2001) 781–786

Best regards,
Andrea

>
> Hi all
> The wafer orientation is 100.
>
> Thank you
reply