Mike,

H2O2 @ 50c

Brent

Michael Cooke wrote:
> Dear all,
>
> I was wondering if there is a safer etch for Titanium which I haven't
> come across which doesn't involve HF or HF as a biproduct. Ideally it
> should be done at room temp.
>