durusmail: mems-talk: removing sticky adhesive
removing sticky adhesive
2008-03-18
2008-03-18
2008-03-18
2008-03-20
2008-04-03
2008-03-21
2008-03-21
removing sticky adhesive
Brad Cantos
2008-03-21
Vikrant,

Something you might try instead of standard cellophane tape is plater's
tape.  It is made of kapton and has a low tack adhesive that works for
masking during plating operations, and also for some etches if they are not
too aggressive.

Brad Cantos


On 3/18/08 7:03 AM, "Vikrant A. Chaudhari :)"  wrote:

> hello,
>
> is there a way to remove sticky adhesive, which is left over after a
> cellotape is removed. we are using cello tape for masking while etching
> SiN, and when cellotape is peeled of the sticky glue is left over. Is
> there a better way to remove it with out scrubbing?
reply