If i don't know false, it should be AuGe Alloy that annealed 1 minute at 480 oC using rapit thermal processor.... Best Regards. Tolga YELBOGA Project Engineer Nanotechnology Researh Center Bilkent University Bilkent, Ankara 06800 TURKEY Voice: 90-312-290-1020 http://www.nanointurkey.com http://www.nanotam.bilkent.edu.tr -----Original Message----- From: vaibhav mathur [mailto:kingvaibhav@hotmail.com] Sent: Thursday, April 10, 2008 8:35 AM To: mems-talk@memsnet.org Subject: [mems-talk] n-type AlGaAs ohmic contacts hi all, can someone please suggest the optimum metal sequence and annealing recipe to form ohmic contacts directly on n-type AlGaAs? regards Vaibhav Mathur PHOTONICS CENTER UMass,Lowell