durusmail: mems-talk: positive tone in AZ5214E image reversal process
positive tone in AZ5214E image reversal process
2008-04-26
2008-04-26
2008-04-26
2008-04-26
2008-04-28
2008-04-30
2008-04-27
positive tone in AZ5214E image reversal process
basar bolukbas
2008-04-26
Hello.
Your basic process details not very bad expect flood-e time.
In order to get negative wall profile you can try 2s. first exposure and
8s.flood exposure with 8mW/cm.
reply