Hi, If you want deposit 20 micron only best suitable way is electroplating. But its not advisable to go for electroplating with gold/platinum in terms of cost. Normally Cu/Ni cane deposited easily with above method. If you are more specific why you are using W may be senior members of the group can help you. Kallempudi Sreenivasa Saravan PhD student, Electronics Engineering, 1054, FENS, Sabanci University, Orhanli, 34956, Tuzla, Istanbul, Turkey. -Hi all, i need to deposit about 20um of any metal on tungsten. Could someone suggest a metal which have good adhesion to tungsten and an appropriate deposition technique ? For my understanding Titanium deposited by electrodeposition should work fine, but i don't have a big experience. Many thanks, Andrea