Hi, everyone, Can anybody please tell me how to improve the sticking of PMMA on Si O2 surface? I am trying to etch a trench of ~50 nm wide and 15 nm deep in the SiO2 layer using HF but the PMMA lift off from the surface when I dip the wafer into HF solution.Any comment is greatly appreciated. Thanks. Jie Liu Rice University