Tell me more about the critical dry procedure. I manufacture vacuum driers and anti stiction coating equipment. I may have a suggestion. Bill Moffat -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Ramakrishna Kotha Sent: Thursday, June 26, 2008 12:34 AM To: mems-talk@memsnet.org Subject: [mems-talk] Critical Dry Hi, I am performing critical dry to release a parallel plate structure, which has SiO2 as a sacrificial layer After removing the sacrifical layer-SiO2 with BOE, then the device is transffered to DI Water and then to Acetone in the critical dry chamber. After performig critical dry process using Polaron-CPD 7501 tool, all the structures are damaged (due to stiction problem). Can anyone, suggest me the accurate process to perform critical dry. Thanks in advance Rama _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk