What do you mean about "that this protective film only takes about an hours in KOH 40% at 60ºC"? 2008/7/4, Anahí Weinstock: > Hi > I´m using black wax as wet etching protector. In bibliografy it is > dissolved in toluene and cured at 100 ºC in oven for 1 hs, then after > being deposited on the wafer. The problem is that this protective film > only takes about an hours in KOH 40% at 60ºC. > Someone has experience what are the optimal conditions for working with > this material? > Thanks > Anahí -- Best regards, Yours sincerely Fei Wang ______________ State Key Lab of Transducer Technology, Shanghai Institute of Microsystem and Information Technology, Chinese Academy of Sciences 865 Changning Road, Shanghai 200050, China Email:wangfeiustc@gmail.com Tel:0086-21-62511070 ext.5468