durusmail: mems-talk: Ni plating on Au film
Ni plating on Au film
2008-07-16
2008-07-18
2008-07-20
Ni plating on Au film
Moshe
2008-07-20
Nickel strike is a thin  intermediate film that made from 210 gr/ liter Nickel
Chloride , 90ml/liter HCl - and the rest is DI water .
This  intermediate make the adhesion bettwen the metal and the Nickel.
It usually use to make adhesion between stainless steel and Nickel.




reply