I would try a proprietary alkaline gold stripping solution like it is sold by companies as Technic / Rohm and Haas / MECO or Enthone (I'm not trying to make this a commercial) but these goldstripping solutions barely attack nickel, so I expect nearly no attack on the Mo as well. However I never tried it out. Good luck, Harry