durusmail: mems-talk: Si Etch Initiation Failure
Si Etch Initiation Failure
2008-07-26
2008-07-26
2008-07-27
2008-07-28
2008-07-28
2008-08-03
Si Etch Initiation Failure
Muk Mei Yu
2008-07-28
Hi Shay,

Sorry to mention that 'BOE prior to etch' is already incorporated in my process,
but yet I still encounter etch initiation failure. Do you mean fluorine
contamination will prohibit the etching?

Thanks,
Muk

reply