wafer bow spec
2008-10-02
2008-10-02
2008-10-02
2008-10-03
wafer bow spec
Laura Malatto
2008-10-02
It´s about  0.06 um

Laura

John-Rolf Oakley escribió:
> Hello,
>
> I am having trouble keeping vacuum on some wafers and I was wondering if
anyone could tell me what the SEMI standard for wafer bow is on 6", 675um,
single flat, single side polished, <100>, P type Si?
>
> Thanks