There are a variety of glass pastes that can be screen printed that will fire to a thickness of 30u or greater. They come in a wide variety of melting and firing temperatures and Tce values (which will have a big effect at that thickness). Most have other components besides SiO2 to reduce the firing temperature and are designed for specific purposes. What do you have above and below it? -- Tom Rust Nanochip Inc (510) 339-6263 (510) 339-9636 FAX (510) 912-4662 cell http://www.nanochip.com