Increase exposure a lot more. Develop with AZ 1:3. It should work. Good luck On Tue, Dec 2, 2008 at 12:05 PM, Hyun C Jungwrote: > This is my parameters for AZ 9260. > > 1. Spin coat AZ 9260 at 3000 rpm for 1 min. > 2. Soft bake for 90s > 3. Expose 15s i-line4 > 4. Develop 3 min in AZ 400k 1:4