Hi José, Just a thought... Is there any electrical connection between your SOI layer and the substrate? If not, your SOI layer may be charging up and your bias at the etched surface could be far different from any bias you've set on the handle wafer. Best, Dean Hopkins dean-hopkins@sbcglobal.net (408) 429-0501