durusmail: mems-talk: conductive su-8
conductive su-8
2009-01-18
2009-01-19
conductive su-8
shay kaplan
2009-01-19
Vaibhav

There is a resist the is electrodeposited called Eagle 2000. try it.

shay

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of vaibhav mathur
Sent: Monday, January 19, 2009 12:00 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] conductive su-8

hi, I am looking to use some kind of conductive photoresist. I have heard of
people mixing silver nanoparticles, or polyaniline with su-8 to make it
conductive.if someone has any experience, with this, please help me, as I
need one urgently. Is it possible to buy something like this in the market??

regards

vaibhav
reply