Hi Roger, Would you please specify the voltage that you used for bonding? Is that the same as Gareth mentioned? Thank you. On Thu, Feb 12, 2009 at 5:31 PM, Roger Shilewrote: > The first time I did an anodic bond I used a hot plate and DC power > supply that were lying around. Just to be cute I used a coat hanger as > an anode. > > The bonds were as good as what I get now using a very high priced > commercial bonder. I still get a lot of laughs over that hot plate and > coat hanger. > > Roger -- Jingru