We are trying to spincoat Nusil CF19-2186 elastomer. We are facing problems
because the liquid is highly viscous and I think it starts to cure while we
are trying to degass it. The mixing of the base and the curing agent also
causes a lot of bubbles, so we think it is essential that we degass it
before spincoating. We are also trying to coat without degassing with mixed
results.

Any suggestions?.