Bearing holes in pyrex/glass wafers
Xiaoguang Liu
2009-05-02
Hi Jim
Can the abrasive powder blasting be done in house or you send it out
to some service providers?
Thanks,
Leo

On Fri, May 1, 2009 at 11:19 PM,   wrote:
> TJ,
>
> I always liked micro abrasive powder blasting for quick turn prototype work.
>
> Jim
>
>

--
Xiaoguang "Leo" Liu
Birck Nanotechnology Center,
Purdue University,
1205 W.State Street, West Lafayette, IN, 47906 USA