Evelyn, Lift off profile is generally regarded as an over hang deliberately created in the resist profile. So when the metal is deposited it can not cover the overhanging resist side wall. See example, in attachment. Bill Moffat. -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of saravan kallempudi Sent: Sunday, May 03, 2009 4:06 AM To: mems-talk@memsnet.org Subject: Re: [mems-talk] Lift-off Profile Dear Evelyn, For lift off the best suited one is sputter deposition and it is the one which makes an conformal layer. The coverage depends on the type of PR you are going to use. In order to perform a successful liftoff using image reversal process, the thickness of PR should be atleast 2 times of the metal thickness. --Saravan