Hello, If this is just a temporary fixture, you may be able to use photoresist to glue the backside of your silicon wafer to your glass disk. If you get to a point in which you don't need the glass disk anymore, you should be able to remove the resist using acetone to unglue your Si wafer from the glass disk. Hope this helps. Tony P On Thu, May 7, 2009 at 9:43 AM, Maria Matschukwrote: > Dear all, > > I need to fix a Silicon wafer (coated with resist) to a glass disk. Does anyone have experience with some kind of glue (or another method)? > > Kind Regards > > Maria -- Tony Price Department of Electrical Engineering University of South Florida 4202 E. Fowler Avenue, ENB-118, Tampa, FL, 33620 Office: ENG 108 Phone: (813) 396-9310