durusmail: mems-talk: Curing of PDMS
Curing of PDMS
2009-05-15
2009-05-15
2009-05-15
2009-05-18
Curing of PDMS
DEBASHIS MAJI
2009-05-15
Hi all,

I would like to know whether there is any difference in the curing
of PDMS if it done using a vacuum oven ( i.e. by convection curing ) or
over a hot plate( conduction curing ) with a vacuum system. Is there any
particular temperature difference in the two process that might be necessary
for complete curing of the PDMS ? If so how much?  I think that the vacuum
oven ( by convection ) may need a greater temp as compared to the other one.

Any kind of help shall be highly appreciated.

Thanks and Regards,

Debashis Maji, JRF,
School of Medical Science & Technology,
IIT Khargpur, India - 721302
reply