Hi Ben Pepin, The thickness depends on the material you want to deposit on a given substrate and the quality of deposit you would like to achieve. I have deposited about 10 microns gold on a silicon substrate patterned with a Chromium-Gold seeding. There might be a thicker deposit than what I have mentioned but then again it depends various process variables, coat quality, material deposited and the substrate. Regards, Prasanna On Mon, May 25, 2009 at 6:21 PM, Ben Pepinwrote: > Hello, > > I am an undergraduate research student at Mizzou and was wondering how > thick > of a coat you can achieve from electroplating? I am trying to get as thick > of a coat as possible and would appreciate any tips or suggestions. > > Thanks, > Ben Pepin > bjp3z4@mizzou.edu