Hi Dave,
It is not a thin W film.

Thanks,
Andrea

> Hi Andrea,
> You can plate Ni or NiCo on W assuming it's thick enough.
> If it's a thin W film < 300nm or so, you'd have to coat it first with
> sputtered Ni, or Au.
> Dave