Hi You should do first a cyclic voltammogram and look for deposition peak .. You will be able then to find from that the right values for potential Petru On Thu, Jun 4, 2009 at 5:24 PM, Ben Pepinwrote: > Hello, > > I am trying to electroplate copper sulfate onto a piece of titanium that has > a surface area of about 0.003 cm^2. I am wondering if anyone knows what type > of power supply I should use and how much current I should use. > > Thanks, > Ben Pepin